Nano-meter scale plasticity in KBr studied by nanoindenter and force microscopy
Published online by Cambridge University Press: 31 January 2011
Abstract
The early stages of plasticity in KBr single crystals have been studied by means of nanometer-scale indentation in complementary experiments using both a nanoindenter and an atomic force microscope. Nanoindentation experiments precisely correlate indentation depth and forces, while force microscopy provides high-resolution force measurements and images of the surface revealing dislocation activity. The two methods provide very similar results for the onset of plasticity in KBr. Upon loading we observe yield of the surface in atomic layer units which we attribute to the nucleation of single dislocations. Unloading is accompanied by plastic recovery as evident from a non-linear force distance unloading curve and delayed discrete plasticity events.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 2009
References
- 3
- Cited by