Abstract
Humidity and temperature control accessories for Hysitron Triboscope have been developed to study the environmental influence on in situ properties of drying coatings. Mechanical properties of drying poly (vinyl alcohol) (PVOH) and poly (vinyl pyrrolidone) (PVP) coatings on silicon wafer were measured under different humidities. The modulus results were compared with outputs of elastic, plastic and viscoelastic theories of indentation testing.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 2000
References
REFERENCES
1.
Gutoff, E. B. and Cohen, E. D., Coating and Drying Defects: Troubleshooting Operating Problems, (J. Wiley and Sons, New York, 1995).Google Scholar
2.
Errede, L. A., Heinrich, P. J. and Tiers, G. V. D., J. Appl. Polym. Sci., 54, 669 (1994).Google Scholar
4.
Cairncross, R. A., Jeyadev, S., Dunham, R. F., Evans, K., Francis, L. F. and Scriven, L. E., J. Appl. Polym. Sci., 58, 1279 (1995).Google Scholar
9.
Gerberich, W. W., Yu, W., Kramer, D., Strojny, A., Bahr, D., Lilleodden, E. and Nelson, J., J. Mater. Res., 13, 421 (1998).Google Scholar
10.
Cheng, L., Scriven, L. E. and Gerberich, W. W., in Proceeding of the 4th World Congress on Computational Mechanics, (Buenos Aires, Argentina, 1998).Google Scholar
11.
Cheng, L., Xia, X., Yu, W., Scriven, L. E. and Gerberich, W. W., J. Polym. Sci.: Part B: Polym. Phys., 37 (1999).Google Scholar
12.
Cheng, L., Scriven, L. E. and Gerberich, W. W., in Fundamentals of Nanoindentation and Nanotribology, edited by Moody, N.R., Gerberich, W.W., Burnham, N. and Baker, S. P. (Mater. Res. Soc. Proc. 522, Warrendal, PA
1998), 193.Google Scholar
14.
Dibbern-Brunelli, D., Atvars, T. D., Joekes, I. and Barbosa, V. C., J. Appl. Polym. Sci., 69, 645 (1998).Google Scholar