No CrossRef data available.
Article contents
Effect of Post-Metallization Hydrogen Annealing on C-V Characteristic of Zirconia Grown Using Atomic Layer Deposition
Published online by Cambridge University Press: 11 February 2011
Abstract
Substantial amount of fixed charge present in most of the alternative gate dielectrics gives rise to large shifts in the flat-band voltage (VFB) and charge trapping and de-trapping causes hysterectic changes on voltage cycling. Both phenomena affect stable and reliable transistor operation. In this paper we have studied for the first time the effect of post-metallization hydrogen annealing on the C-V curve of MOS capacitors employing zirconia, one of the most promising gate dielectric. Samples were annealed in hydrogen ambient for up to 30 minutes at different temperatures ranging from room temperature to 400°C. C-V measurements were done after annealing at each temperature and the hysteresis width was calculated from the C-V curves. A minimum hysteresis width of ∼35 mV was observed on annealing the sample at 200°C confirming the excellent suitability of this dielectric.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 2003