Measurement of Long Range Order in the γ’ Phase of Nickel-Base Superalloys
Published online by Cambridge University Press: 06 March 2019
Abstract
The long range order parameter (S) has been measured at room- temperature on the γ’ phase extracted from IN-731 and alloys 713C and 713LC by x-ray diffraction techniques. Measurements were obtained from specimens of IN-731 and alloy 713LC in the as-cast condition and after long time rupture testing. The alloy 713 c specimens were in the as-cast and high temperature heat treated conditions.
It was found that long range order in the γ’ phase of IN-731 and alloy 713LC was changed very little after long time rupture testing, and after high temperature heat treatment in the case of alloy 713C.